INCOLOY® alloy 27-7MO

INCOLOY-Alloy-27-7MO

INCOLOY Alloy 27-7MO (UNS S31277) Product Introduction

Chemical Composition

ElementComposition (%)
Nickel (Ni)26.0 – 28.0
Chromium (Cr)26.0 – 28.0
Molybdenum (Mo)6.0 – 7.0
Nitrogen (N)0.25 – 0.30
Iron (Fe)Balance
Copper (Cu)1.5 – 2.5
Manganese (Mn)1.0 max
Silicon (Si)0.5 max
Carbon (C)0.010 max
Phosphorus (P)0.030 max
Sulfur (S)0.010 max

Mechanical Properties

PropertyValue
Tensile Strength, ksi (MPa)115 (795) min
Yield Strength (0.2% offset), ksi (MPa)55 (380) min
Elongation (% in 2 inches)40 min
Hardness, Brinell (HB)255 max

Performance at Different Temperatures

Temperature RangePerformance
Room TemperatureExcellent mechanical properties and corrosion resistance.
Elevated Temperatures (up to 1000°F / 538°C)Maintains strength and oxidation resistance.
Low TemperaturesRetains toughness and ductility down to cryogenic temperatures.

Industry Applications

Industry SectorApplications
Oil and GasDownhole equipment, subsea pipelines.
PetrochemicalHeat exchangers, chemical processing equipment.
MarineOffshore platforms, seawater handling systems.
Power GenerationCondensers, boiler components.

Shape, Size, and Production Standards

Product FormShapes AvailableSizes AvailableProduction Standards
SheetsPlates, SheetsVarious thicknessesASTM B688, ASTM B709
BarsRound bars, hexagonal barsDiameter rangeASTM B805
Tubes/PipesSeamless tubes, welded pipesVarious dimensionsASTM B690, ASTM B775

Standards and Corresponding Grades

Country/RegionStandard/Grade
USAUNS S31277
Europe1.4529
GermanyX1NiCrMoCuN20-18-7
FranceZ1NCDU20.18.06Az

Welding, Processing, Polishing, Heat Treatment

ProcessDetails
WeldingExcellent weldability using TIG, MIG methods.
ProcessingCold and hot forming processes. Machinable with standard methods.
PolishingAchieves smooth finishes suitable for sanitary applications.
Heat TreatmentSolution annealing at 2100°F (1150°C) followed by rapid quenching.

Cold Processing, Advantages, and Disadvantages

AspectDetails
Cold ProcessingExcellent formability and cold workability.
AdvantagesHigh resistance to chloride-induced stress corrosion cracking. Good mechanical properties over a wide temperature range.
DisadvantagesHigher initial cost compared to standard stainless steels. Requires expertise in welding to prevent sensitization.

Similar Products

Product NameComparison
Alloy 926 (UNS N08926)Higher molybdenum content, similar applications in aggressive environments.
Alloy 254 SMO (UNS S31254)Higher chromium and molybdenum content, excellent resistance to pitting and crevice corrosion.

Comparison of Similar Products

Property/FeatureINCOLOY Alloy 27-7MO (UNS S31277)Alloy 926 (UNS N08926)Alloy 254 SMO (UNS S31254)
Nickel Content (%)26.0 – 28.024.0 – 26.018.0 – 20.0
Chromium Content (%)26.0 – 28.019.0 – 21.019.5 – 20.5
Molybdenum Content (%)6.0 – 7.06.0 – 7.06.0 – 6.5
Copper Content (%)1.5 – 2.51.5 – 3.00.5 – 1.0
Nitrogen Content (%)0.25 – 0.300.15 – 0.250.18 – 0.22
Tensile Strength (ksi)115 min100 min100 min
Yield Strength (ksi)55 min45 min45 min
Elongation (%)40 min40 min35 min
Resistance to SCCHighHighHigh
Typical ApplicationsOil and gas, petrochemical, marineChemical processing, marineChemical processing, marine

This structured presentation provides a detailed overview of INCOLOY Alloy 27-7MO (UNS S31277), encompassing its chemical composition, mechanical properties, performance characteristics at different temperatures, industry applications, available shapes and sizes, production standards, welding and processing capabilities, as well as the advantages, disadvantages, and comparable products. Each section is organized into tables to ensure clarity and accessibility of technical specifications and comparisons.