Granica plastyczności (przesunięcie 0,2%), ksi (MPa)
45 (310) min
Wydłużenie (% na 2 cale)
40 min
Hardness, Brinell (HB)
200 max
Wydajność w różnych temperaturach
Zakres temperatury
Wydajność
Temperatura pokojowa
Excellent mechanical properties and corrosion resistance.
Elevated Temperatures (up to 2000°F / 1093°C)
Maintains strength and oxidation resistance.
Low Temperatures
Retains toughness and ductility down to cryogenic temperatures.
Zastosowania branżowe
Sektor przemysłowy
Aplikacje
Przetwarzanie chemiczne
Chemical reactors, sulfuric acid production.
Petrochemical
Heat exchangers, piping systems.
Olej i gaz
Offshore platforms, seawater applications.
Wytwarzanie energii
Boiler components, turbine exhaust systems.
Shape, Size, and Production Standards
Formularz produktu
Dostępne kształty
Dostępne rozmiary
Standardy produkcyjne
Pościel
Talerze, prześcieradła
Various thicknesses
ASTM B688, ASTM B709
Słupy
Round bars, hexagonal bars
Diameter range
ASTM B805
Rury/Rury
Seamless tubes, welded pipes
Various dimensions
ASTM B690, ASTM B775
Standards and Corresponding Grades
Kraj/region
Standard/Grade
USA
UNS N08028
Europe
1.4563
Niemcy
X1NiCrMoCu31-27-4
Francja
Z1NCDU31-27-03
Welding, Processing, Polishing, Heat Treatment
Proces
Detale
Spawalniczy
Excellent weldability using TIG, MIG methods.
Processing
Cold and hot forming processes. Machinable with standard methods.
Polerowanie
Achieves smooth finishes suitable for sanitary applications.
Obróbka cieplna
Annealing at 2050°F (1121°C) followed by rapid quenching.
Cold Processing, Advantages, and Disadvantages
Aspekt
Detale
Cold Processing
Excellent formability and cold workability.
Zalety
High corrosion resistance in a wide range of aggressive environments. Good mechanical properties at elevated temperatures.
Niedogodności
Higher initial cost compared to standard stainless steels. Requires expertise in welding to prevent sensitization.
podobne produkty
Product Name
Porównanie
Inconel 625 (UNS N06625)
Lower nickel content, similar applications in corrosive environments.
Hastelloy C-276 (UNS N10276)
Higher molybdenum content, superior resistance to pitting and crevice corrosion.
This structured presentation offers a detailed overview of INCOLOY Alloy 028 (UNS N08028), encompassing its chemical composition, mechanical properties, performance characteristics at different temperatures, industry applications, available shapes and sizes, production standards, welding and processing capabilities, as well as the advantages, disadvantages, and comparable products. Each section is organized into tables to ensure clarity and accessibility of technical specifications and comparisons.