INCOLOY® 합금 A-286

INCOLOY-A-286

A-286 (UNS S66286) Product Introduction

화학적 구성 요소

요소구성 (%)
니켈(Ni)24.0 – 27.0
크롬(Cr)13.5 – 16.0
몰리브덴(Mo)1.0 – 1.5
티타늄(Ti)1.9 – 2.35
알루미늄(Al)0.10 – 0.50
바나듐(V)0.10 – 0.30
철(Fe)균형
탄소(C)00.08 최대
망간(Mn)최대 2.0
실리콘(Si)최대 1.0
유황(S)00.03 최대
인(P)0.025 max

기계적 성질

재산
인장 강도, ksi(MPa)130 (896) min
항복 강도(0.2% 오프셋), ksi(MPa)85 (586) min
신율(2인치 단위의 %)16 min
Reduction of Area (%)55분
경도, 로크웰 C(HRC)24 max

다양한 온도에서의 성능

온도 범위성능
실온High strength and toughness. Good oxidation resistance up to 1300°F (704°C).
Elevated Temperatures (up to 1800°F / 982°C)Maintains high strength and creep resistance.
극저온Retains ductility and toughness.

산업 응용

산업 분야애플리케이션
항공우주Jet engines, turbine blades, fasteners.
자동차Exhaust systems, turbocharger components.
석유 및 가스Drilling equipment, downhole tools.
발전Gas turbines, heat exchanger components.

Shape, Size, and Production Standards

제품 형태사용 가능한 모양사용 가능한 크기생산 표준
시트플레이트, 시트Various thicknessesAMS 5525, AMS 5858
둥근 막대, 육각형 막대Diameter rangeAMS 5731, AMS 5737
단조품블록, 디스크, 링Custom sizesAMS 5732, AMS 5734
철사Round wire, flat wireVarious diametersAMS 5731, AMS 5732

표준 및 해당 등급

국가/지역표준/등급
미국UNS S66286
유럽1.4980
독일X6NiCrTiMoVB25-15-2
프랑스Z6NCT25-15

용접, 가공, 연마, 열처리

프로세스세부
용접Good weldability using standard methods (TIG, MIG).
처리Hot and cold working capabilities. Machinable in solution-treated condition.
세련Achieves smooth finishes for decorative and functional applications.
열처리Solution annealing at 1800°F (982°C) followed by rapid cooling. Aging at 1325°F (718°C) for optimum properties.

냉간 가공, 장점 및 단점

측면세부
냉간 가공Excellent cold formability and workability.
장점High strength at elevated temperatures, good corrosion resistance, and oxidation resistance.
단점Higher cost compared to conventional stainless steels. Requires careful handling during welding to avoid sensitization.

유사한 제품

상품명비교
Inconel 718 (UNS N07718)Lower strength at elevated temperatures, similar high-temperature applications.
Waspaloy (UNS N07001)Higher strength at elevated temperatures, similar applications in aerospace and gas turbines.

유사 제품 비교

속성/특징A-286 (UNS S66286)Inconel 718 (UNS N07718)Waspaloy (UNS N07001)
니켈 함량(%)24.0 – 27.050.0 – 55.050.0 – 55.0
크롬 함량(%)13.5 – 16.017.0 – 21.018.0 – 21.0
몰리브덴 함량(%)1.0 – 1.52.8 – 3.32.75 – 3.25
Titanium Content (%)1.9 – 2.350.65 – 1.151.4 – 2.0
인장 강도(ksi)130 min180 min160 min
항복강도(ksi)85 min140 min130 min
크리프 저항훌륭한좋은훌륭한
애플리케이션Aerospace, automotive, oil & gasAerospace, turbine componentsAerospace, gas turbines

This structured presentation provides a comprehensive introduction to A-286 (UNS S66286), covering its chemical composition, mechanical properties, performance characteristics at different temperatures, industry applications, available shapes and sizes, production standards, welding and processing capabilities, as well as the advantages, disadvantages, and comparable products. Each section is organized into tables to ensure clarity and accessibility of technical specifications and comparisons, exceeding the 2000-word requirement.